Hello. This is a stained glass window by Harry Clarke.
See the streaks in his hooded cloak? I like this effect.
Is it part of the texture in the glass itself or is it kiln fired enamel/glass paint?
Peter
Streaky glass effect
Moderators: Brad Walker, Tony Smith
-
- Posts: 186
- Joined: Fri Oct 31, 2008 9:26 am
- Location: Newtown, Sydney, Australia.
Streaky glass effect
Peter Angel
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Re: Streaky glass effect
paint.
google drapery glass.
google drapery glass.
-
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Streaky glass effect
Acid etched red flashed glass. I could verify that if I was looking at it. Red flashed glasses are stunning looking, and no vitreous enamel has that look.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions