Streaky glass effect

Post by Peter Angel »

Hello. This is a stained glass window by Harry Clarke.
tumblr_mk2nmiqjTP1rqygz0o1_500.jpg
See the streaks in his hooded cloak? I like this effect.

Is it part of the texture in the glass itself or is it kiln fired enamel/glass paint?

Peter
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Streaky glass effect

Post by Marty »

paint.

google drapery glass.
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Streaky glass effect

Post by Bert Weiss »

Acid etched red flashed glass. I could verify that if I was looking at it. Red flashed glasses are stunning looking, and no vitreous enamel has that look.