I want to slump a piece of 14"x7" 3/8" glass into a curved mold, and create a flat triangular spot near the top, so I can glue another piece to it. I tried a test, and used a fibre board for the flat spot. Went to 1245 F, and it was close to what I'd want to achieve. But the fibre board seems toxic to my lungs, as does fibre paper. I'd like to find something that would be more user friendly. Possibly a ceramic tile with ludo on top....? I need to do 15 of these when I get the concept down.
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: slumping glass into a mold, and also creating a flat spo

Post by Bert Weiss »

Brad sells a stiff thin board. I think it is 110J You still have to burn it out, but it is more durable than the 970 papers, so there would be fewer burnout fumes in the long run.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Marian
Posts: 71
Joined: Mon Dec 06, 2004 5:37 pm
Location: Big Island Hawaii
Contact:

Re: slumping glass into a mold, and also creating a flat spo

Post by Marian »

Did you try to cold work the flat spot with with a grinder or abrasive pad? Are you slumping the flat spot on the bottom of your mold or balancing a tile on top while you slump? Ceramic tile is inert, use kiln wash.
Susanbuckler
Posts: 68
Joined: Tue Aug 18, 2009 10:31 pm

Re: slumping glass into a mold, and also creating a flat spo

Post by Susanbuckler »

Bert
What is 210J? Can it be used like fiber paper to dam glass? I found it on Brad's website but I do not see enough info for me to understand what it is and how to use it. Thanks
Susan
Susan Buckler
Woodstock, NY
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: slumping glass into a mold, and also creating a flat spo

Post by Bert Weiss »

Susanbuckler wrote:Bert
What is 210J? Can it be used like fiber paper to dam glass? I found it on Brad's website but I do not see enough info for me to understand what it is and how to use it. Thanks
Susan
It is a thin, stiff, board. I have messed around with it, but it is not one of my usual materials, in the studio. Ask Brad, if you have more questions about it.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: slumping glass into a mold, and also creating a flat spo

Post by Morganica »

jerry keller wrote:I want to slump a piece of 14"x7" 3/8" glass into a curved mold, and create a flat triangular spot near the top, so I can glue another piece to it. I tried a test, and used a fibre board for the flat spot. Went to 1245 F, and it was close to what I'd want to achieve. But the fibre board seems toxic to my lungs, as does fibre paper. I'd like to find something that would be more user friendly. Possibly a ceramic tile with ludo on top....? I need to do 15 of these when I get the concept down.
Kilnsafe + respiratory-safe can be a bit difficult to achieve. I was going to suggest simply getting some plaster, dolloping it on your wet bisque/ceramic mold (it won't stick if the mold is dry), and shaping it as needed, but you'll still need a respirator.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: slumping glass into a mold, and also creating a flat spo

Post by Stephen Richard »

I think ludo would stick to the glass