Hi, what does everyone recommend as a good adhesive to attach findings?
Thanks
Cherie
Attaching findings to pendants
Moderators: Brad Walker, Tony Smith
-
Cherie Knopf
- Posts: 14
- Joined: Tue Apr 23, 2013 8:37 pm
- Location: Morgan Hill, California
- Contact:
Re: Attaching findings to pendants
I use E6000, it works and is simple to apply.
Couple of things to watch:
For pendants, roughen up area on glass plus on bail if bail is one of those that looks like a flat metal strip with a loop on top. Not necessary if you use Aanraku type bails, these are slightly concave. Sometimes I hold bail and pendant together with a large spring clip, depends on the design of both.
Clean glue area. I use acetone, I think many people use alcohol.
Do not touch glued pieces for 24 hours.
If possible, keep close to a heat source, so it warms (not heat) glued pieces.
Enter e6000 in search, pretty sure you'll get lots of information from previous posts on this board, has been discussed often.
I like it because results are good and is pretty easy to use. Cures clear. Very, very few failures.
Best regards, seachange
Couple of things to watch:
For pendants, roughen up area on glass plus on bail if bail is one of those that looks like a flat metal strip with a loop on top. Not necessary if you use Aanraku type bails, these are slightly concave. Sometimes I hold bail and pendant together with a large spring clip, depends on the design of both.
Clean glue area. I use acetone, I think many people use alcohol.
Do not touch glued pieces for 24 hours.
If possible, keep close to a heat source, so it warms (not heat) glued pieces.
Enter e6000 in search, pretty sure you'll get lots of information from previous posts on this board, has been discussed often.
I like it because results are good and is pretty easy to use. Cures clear. Very, very few failures.
Best regards, seachange
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Attaching findings to pendants
Make sure to always use fresh E6000. I always squeeze out and discard an inch or so before using it.
-
Cherie Knopf
- Posts: 14
- Joined: Tue Apr 23, 2013 8:37 pm
- Location: Morgan Hill, California
- Contact:
Re: Attaching findings to pendants
I had tried a little tube of the E6000 but it just seems so stringy I had a harder time applying without getting glue all over everything. Maybe just user error 
Re: Attaching findings to pendants
Go to Barry Kaiser's website. He has a very clear tutorial on it.
KaiserGlass.com (I think)
KaiserGlass.com (I think)
Re: Attaching findings to pendants
It can be stringy. I use the "toothpick and twirl" method. Works just fine for me - no waste, and I can control by sight the amount I want.
-
Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: Attaching findings to pendants
Thanks Guy,GuyKass wrote:Go to Barry Kaiser's website. He has a very clear tutorial on it.
KaiserGlass.com (I think)
Yep, E-6000 is a (within reason) never fail adhesive if used properly. In addition it is cheap and easy to use (correctly).
Barry
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns