Post by Laurie Spray »

I have just completed a new tutorial on the "Pattern Bar Flow Technique". Thought I would share it here. It is too much fun! We have just barely dented the surface on the fun possibilites of this technique and I am loving it!
http://www.igrowhydro.com/fusedglassart ... hnique.pdf
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: New tutorial

Post by Barry Kaiser »

Cool look and so easy!!

Barry
Gail L
Posts: 18
Joined: Mon Jun 13, 2005 9:25 am
Location: South Florida

Re: New tutorial

Post by Gail L »

Going to try it with my 12 !/2" SS round from Laurie !
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: New tutorial

Post by JestersBaubles »

Thank you for sharing the info, Laurie. I particularly like the design of the piece in the very last picture (love the color purple).

Dana W.
Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: New tutorial

Post by Laurie Spray »

These pictures are just some starters learning the weights and fusing programs. It has opened my mind to lots and lots of new possibilities! I have had a HUGE email response today from customers that are so excited! Really fun! Soon I will have all the weights calculated to make it even easier! I will add more pictures to the tutorial on our site as they come out of the kilns. :D
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Eric Baker
Posts: 51
Joined: Thu May 20, 2004 9:19 am
Location: Owasso, OK

Re: New tutorial

Post by Eric Baker »

Those are fun, and a lot of possibilities exist. I had a similar idea a few years back with some scrap pattern bar pieces, but never followed up--just left it sitting in the 'try it someday' pile.

Now I'll brush off the dust and go with the 'flow'.

Thanks for sharing, Laurie.


warm regards,

Eric
Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: New tutorial

Post by Laurie Spray »

Here is a set of pattern bars that were made of old bullseye pattern bars that I was not crazy about. pic is of 4 sets of them after I had done the "flow" in one of our stainless steel rings. Having way to much fun here! This one sold right out of the slump still warm!

image.jpg
image.jpg
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: New tutorial

Post by JestersBaubles »

Laurie Spray wrote:Here is a set of pattern bars that were made of old bullseye pattern bars that I was not crazy about. pic is of 4 sets of them after I had done the "flow" in one of our stainless steel rings. Having way to much fun here! This one sold right out of the slump still warm!
Beautiful, Laurie.

I ordered a new tile saw (MX-370exp) that should arrive early this next week. Can't wait to get cutting!

Dana W.
Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: New tutorial

Post by Laurie Spray »

I just got a "brutus". i Love it!!!
http://www.amazon.com/QEP-61024-24-Inch ... s+tile+saw
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: New tutorial

Post by Laurie Spray »

I just got a "brutus". i Love it!!!
http://www.amazon.com/QEP-61024-24-Inch ... s+tile+saw
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Mark Wright
Posts: 49
Joined: Mon Dec 13, 2010 12:43 pm
Location: Raleigh, NC

Re: New tutorial

Post by Mark Wright »

This is great fun!
Thanks Laurie.
Image
Image
Eryc F.
Posts: 50
Joined: Sun Apr 28, 2013 8:29 am
Location: Canton, MA
Contact:

Re: New tutorial

Post by Eryc F. »

Mark that's great!!!! Well done!

I'm going to start playing with bars over the summer.
Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: New tutorial

Post by Laurie Spray »

Very addictive.........so much fun to do something new!!!!
Thanks for posting the pictures!!
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Post Reply