Re: Density of Spectravue white?

Post by Bert Weiss »

Ferro's website really sucks. Here is info about the xpression series
http://www.ferro.com/Our+Products/Color ... ic+Colors/
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Density of Spectravue white?

Post by Buttercup »

Thanks, Bert. (Thought I'd replied to this but apparently not). I've sent some questions to Sean Weirs who has already sent me some info. I'm awaiting his response to my questions. Jen
Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: Density of Spectravue white?

Post by Peter Angel »

Jen, do you have an update on this?

Pete
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Density of Spectravue white?

Post by Buttercup »

Pete, the samples arrived, very quickly, and as soon as I finish fiddling with artwork I'll unpack them. It was suggested to me that they won't stand the high temperature of soldering but would probably handle flux OK so could I fire the product after assembly. This isn't possible, of course. For a project that isn't copper-foiled and/or leaded and puttied, such as a fused panel, or an already-slumped bowl, it would no doubt be fine. I think that's how others have used it successfully. Also an assembled panel won't fit in the kiln.

The short answer is, I haven't tried them yet but as soon as I do I'll report. Jen