I got a Jen-Ken AF3P Fuse Box 6/4.5 Flex kiln from Kiln Frog. My first kiln. I started out using a Fuseworks microwave kiln.
It came with a little bit of "high fire kiln wash" and it says to apply to kiln shelf (which I already knew to do), and to the kiln bottom. Is this correct? Why would kiln wash need to be applied to the kiln bottom if the posts/feet are used and a kiln washed shelf on top?
Also, I plan on using casting (jewelry) molds and for some reason my shelf wasn't in my box so I will have to have Kiln Frog deal with Jen-Ken this week about that, but anyway, do I put my casting mold on top of a shelf, or just on top of the feet/posts?
I can't find much information on this kiln so if anyone has any tips/additional info, or links that might help me, feel free to share!
also, any links or suggestions as to what firing schedule to try out for my first time with one of these molds?
It came with a little bit of "high fire kiln wash" and it says to apply to kiln shelf (which I already knew to do), and to the kiln bottom. Is this correct? Why would kiln wash need to be applied to the kiln bottom if the posts/feet are used and a kiln washed shelf on top?
Also, I plan on using casting (jewelry) molds and for some reason my shelf wasn't in my box so I will have to have Kiln Frog deal with Jen-Ken this week about that, but anyway, do I put my casting mold on top of a shelf, or just on top of the feet/posts?
I can't find much information on this kiln so if anyone has any tips/additional info, or links that might help me, feel free to share!
also, any links or suggestions as to what firing schedule to try out for my first time with one of these molds?
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Questions for first kiln use
The reason for applying kiln wash to the floor of the kiln is so that if you accidentally drop some glass on the floor or if you have a kiln disaster and glass runs off the shelf it won't harm the bottom of the kiln. You only need to reapply every year or so.krccpht wrote:It came with a little bit of "high fire kiln wash" and it says to apply to kiln shelf (which I already knew to do), and to the kiln bottom. Is this correct? Why would kiln wash need to be applied to the kiln bottom if the posts/feet are used and a kiln washed shelf on top?
Either will work. Most times, I put a couple of short posts on top of the shelf and set the molds on top of that. This allows for air circulation beneath the mold. But most molds fire fine just on the shelf anyway, so if you don't have the posts you'll usually be ok.Also, I plan on using casting (jewelry) molds and for some reason my shelf wasn't in my box so I will have to have Kiln Frog deal with Jen-Ken this week about that, but anyway, do I put my casting mold on top of a shelf, or just on top of the feet/posts?
http://creativeparadise.biz/glass/tutor ... t-tutorialalso, any links or suggestions as to what firing schedule to try out for my first time with one of these molds?
Re: Questions for first kiln use
Thanks Brad! Is glass separator the same thing as kiln wash, and is primer also the same thing?
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Questions for first kiln use
Yes, they're pretty much terms for the same thing.krccpht wrote:Thanks Brad! Is glass separator the same thing as kiln wash, and is primer also the same thing?
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: Questions for first kiln use
and batt wash is the ceramics version
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
You can view my Blog at: http://verrier-glass.blogspot.com/
-
Mike Griffin
- Posts: 23
- Joined: Mon Apr 01, 2013 10:04 pm
- Location: Gelorup, Western Australia
Re: Questions for first kiln use
I've had a couple of small pieces of glass adhere to my kiln washed kiln floor. The trouble is, the floor isn't as smooth as a kiln shelf and the pits can grab hold of molten glass. I'm seriously considering laying down 2-3 mm thick ceramic fibre paper on the floor of the kiln once I start doing pot melts and the like.
Re: Questions for first kiln use
When something does come out quite right, do you typically try to first increase hold times, or increase temperature? I used the guide on that link that was posted above. My mold was similar but had more "slots" in it. They weren't quite "right". Also, can I re-fire these in the mold to correct, or should I just start with a fresh batch?
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: Questions for first kiln use
For my two smaller kilns, I have used 1/8" fiber paper on the floor. I've had the same pieces in there for as long as I've had the kilns.Mike Griffin wrote:I've had a couple of small pieces of glass adhere to my kiln washed kiln floor. The trouble is, the floor isn't as smooth as a kiln shelf and the pits can grab hold of molten glass. I'm seriously considering laying down 2-3 mm thick ceramic fibre paper on the floor of the kiln once I start doing pot melts and the like.
I haven't done that for the "big" kiln yet -- that's a lot of fiber paper!
Dana W.
Re: Questions for first kiln use
When something does come out quite right, do you typically try to first increase hold times, or increase temperature? I used the guide on that link that was posted above. My mold was similar but had more "slots" in it. They weren't quite "right". Also, can I re-fire these in the mold to correct, or should I just start with a fresh batch? They were a little bumpy and not smooth on top, like the glass didn't "melt" all the way, but it was fully fused.
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: Questions for first kiln use
It dependskrccpht wrote:When something does come out quite right, do you typically try to first increase hold times, or increase temperature? I used the guide on that link that was posted above. My mold was similar but had more "slots" in it. They weren't quite "right". Also, can I re-fire these in the mold to correct, or should I just start with a fresh batch? They were a little bumpy and not smooth on top, like the glass didn't "melt" all the way, but it was fully fused.
It really depends upon the piece. Sorry, not very helpful, I know!