Hello,
I ask your advice.
I did strip work , with a lot of clear strip (spectrum 96) full fuse
In the place were two clear strips next each other
I can see the connect line .( I hope you can see it in the image.)
I want to get one "clear" unit
How can avoid it next time,
Can it be fix , in this work
All the best
Osnat
Clear border
Moderators: Brad Walker, Tony Smith
Clear border
- Attachments
-
- image.jpg (36.73 KiB) Viewed 6221 times
-
- image.jpg (31.83 KiB) Viewed 6221 times
Osnat
Osnat glass art
http://www.osnatglassart.co.il
http://www.facebook.com/osnat.menshes#! ... es?sk=wall
Osnat glass art
http://www.osnatglassart.co.il
http://www.facebook.com/osnat.menshes#! ... es?sk=wall
-
The Hobbyist
- Posts: 311
- Joined: Sun Mar 09, 2003 7:09 pm
- Location: Sun City West (NW Phoenix), AZ
- Contact:
Re: Clear border
Cut the clear strips ¼" wide and lay them on top of each other, flat.
Jim
Jim
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
Re: Clear border
You open my mind. So simple .Thank you.
How to wipe out those line?
Thanks
Osnat
How to wipe out those line?
Thanks
Osnat
Osnat
Osnat glass art
http://www.osnatglassart.co.il
http://www.facebook.com/osnat.menshes#! ... es?sk=wall
Osnat glass art
http://www.osnatglassart.co.il
http://www.facebook.com/osnat.menshes#! ... es?sk=wall