Hello,

I ask your advice.
I did strip work , with a lot of clear strip (spectrum 96) full fuse
In the place were two clear strips next each other
I can see the connect line .( I hope you can see it in the image.)
I want to get one "clear" unit

How can avoid it next time,
Can it be fix , in this work

All the best
Osnat
Attachments
image.jpg
image.jpg (36.73 KiB) Viewed 6219 times
image.jpg
image.jpg (31.83 KiB) Viewed 6219 times
The Hobbyist
Posts: 311
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: Clear border

Post by The Hobbyist »

Cut the clear strips ¼" wide and lay them on top of each other, flat.

Jim
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
osnat
Posts: 49
Joined: Wed Oct 21, 2009 10:02 pm
Location: Israel
Contact:

Re: Clear border

Post by osnat »

You open my mind. So simple .Thank you.

How to wipe out those line?

Thanks