HOW to use this mold

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
bothofushk
Posts: 42
Joined: Sat Jan 22, 2005 3:10 pm
Location: East Texas

HOW to use this mold

Post by bothofushk »

Hi all,,I have this mold that this piece is made from,,(NOT MINE) just found this picture on Etsy,,I have NEVER used this mold cause I couldnt figure out to lay up the glass,,could anyone that has used this mold plz show me a piece BEFORE it is fused??? I am just not willing to waste glass unless I have an idea HOW to first use this,,Thanks so much

bothofushk
Attachments
wierd mold.jpg
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: HOW to use this mold

Post by Brad Walker »

Got a photo of the mold?
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: HOW to use this mold

Post by Valerie Adams »

I'm pretty sure the glass is set up just like you see the finished piece, but flat. I'm guessing that's why the maker covered it randomly with frit; they're hiding the seams. Center piece appears to be a triangle with squares butted up on the angles.
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: HOW to use this mold

Post by Morganica »

Is this a candle holder? Or...?
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
bothofushk
Posts: 42
Joined: Sat Jan 22, 2005 3:10 pm
Location: East Texas

Re: HOW to use this mold

Post by bothofushk »

Thanks for all responding,,I will take a photo of the mold,,but it looks just like the piece of glass,,,I really DONT KNOW what to call this mold lol...maybe some kind of nut dish etc....would the glass just be three pieces butted up ???

bothofushk
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: HOW to use this mold

Post by Valerie Adams »

bothofushk wrote:would the glass just be three pieces butted up ???

bothofushk
Yup.
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: HOW to use this mold

Post by Brock »

The question is not how, but why . . .
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: HOW to use this mold

Post by Valerie Adams »

Brock wrote:The question is not how, but why . . .
EXACTLY my thought but I didn't think I could pull off being that snarky. :twisted:
bothofushk
Posts: 42
Joined: Sat Jan 22, 2005 3:10 pm
Location: East Texas

Re: HOW to use this mold

Post by bothofushk »

LOL,,,maybe yall should have ASKED that question BEFORE I bought the damned thing lol...would have bought another mold that I could do ..

thanks

bothofushk
S.TImmerman
Posts: 235
Joined: Wed Nov 25, 2009 9:23 am
Location: San Diego ,Ca

Re: HOW to use this mold

Post by S.TImmerman »

Why not ask the seller of the mold? Please be aware that there are a LOT of "molds" on etsy.com that are not made professionally like the ones sold commercially or by a glass artist. I have seen plenty on that site that will crack glass or just get ingulfed in the glass when slumped.
bothofushk
Posts: 42
Joined: Sat Jan 22, 2005 3:10 pm
Location: East Texas

Re: HOW to use this mold

Post by bothofushk »

Thanks,,,but I bought this from Slumpys...
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: HOW to use this mold

Post by Brad Walker »

bothofushk wrote:Thanks,,,but I bought this from Slumpys...
Quite a few molds that Slumpy's sells don't work very well for slumping. In fact, when I have people come into my studio and ask about problems they're having with a particular mold, more often than not it's a mold they purchased from Slumpy's.

On the positive side, their molds are inexpensive and easy to buy. On the negative, they're not always designed to be the best molds for slumping glass.
seachange
Posts: 223
Joined: Tue Apr 18, 2006 1:19 am

Re: HOW to use this mold

Post by seachange »

hi,

wondering if just butting up the glass will make the pieces pull apart during the firing instead of fusing together?

would a good amount of frit on the seams avoids this?

thanks, seachange
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: HOW to use this mold

Post by Brad Walker »

seachange wrote:hi,

wondering if just butting up the glass will make the pieces pull apart during the firing instead of fusing together?

would a good amount of frit on the seams avoids this?

thanks, seachange
You'll need to use frit or more glass on top to get them to fuse together. Just butting up probably won't work.
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: HOW to use this mold

Post by Valerie Adams »

Brad Walker wrote:
seachange wrote:hi,

wondering if just butting up the glass will make the pieces pull apart during the firing instead of fusing together?

would a good amount of frit on the seams avoids this?

thanks, seachange
You'll need to use frit or more glass on top to get them to fuse together. Just butting up probably won't work.
There are a few designs I've made over the years that rely on just butting the piece up to each other; as long as it's two layers of 3mm, it'll work.
bothofushk
Posts: 42
Joined: Sat Jan 22, 2005 3:10 pm
Location: East Texas

Re: HOW to use this mold

Post by bothofushk »

thanks yall...

bothofushk
seachange
Posts: 223
Joined: Tue Apr 18, 2006 1:19 am

Re: HOW to use this mold

Post by seachange »

Many thanks Brad and Valerie.

Best regards, seachange