Gelflex mold material
Moderator: Brad Walker
-
Barbara Rehus
- Posts: 4
- Joined: Mon May 06, 2013 3:06 pm
Gelflex mold material
Can anyone please tell me where I can buy Gelflex mold material in the US or Canada? Thanks.
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Gelflex mold material
Ed Hoy carries it in smaller quantities. I suspect others do as well.
You can also get larger amounts (or get free samples) from the manufacturer, ACC Silicones: http://www.acc-silicones.com/products/m ... ubber.ashx
You can also get larger amounts (or get free samples) from the manufacturer, ACC Silicones: http://www.acc-silicones.com/products/m ... ubber.ashx
Re: Gelflex mold material
Do you need Gelflex specifically or will any meltable mold material do? I use Elastack, a clear PVC that does pretty much the same thing. Compleat Sculptor sells it, and probably a couple other places.
http://www.sculpt.com/catalog_98/RUBBERS/Elastack.php
There's another one, Instamorph, that looks promising, but I haven't played with it yet. And Vinamold, which is used for museum conservation, is sold by a couple of eBay dealers, although you still must ship from the UK.
http://www.sculpt.com/catalog_98/RUBBERS/Elastack.php
There's another one, Instamorph, that looks promising, but I haven't played with it yet. And Vinamold, which is used for museum conservation, is sold by a couple of eBay dealers, although you still must ship from the UK.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Joe Pfeifer
- Posts: 24
- Joined: Thu May 27, 2010 9:55 pm
Re: Gelflex mold material
I know Milon Townsend has been selling Gelflex too.
http://www.milontownsend.com/contact.html
He also has a great book and DVD on kiln casting
http://thebluemoonpress.com/index.php?m ... ucts_id=36
http://www.milontownsend.com/contact.html
He also has a great book and DVD on kiln casting
http://thebluemoonpress.com/index.php?m ... ucts_id=36
-
Barbara Rehus
- Posts: 4
- Joined: Mon May 06, 2013 3:06 pm
Re: Gelflex mold material
Thank you all for the valuable information.