Fusiing different coe glass in the same firing

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
toolfan88
Posts: 10
Joined: Tue Jun 04, 2013 8:23 pm

Fusiing different coe glass in the same firing

Post by toolfan88 »

Hey. I understand about compatible coe and you cant mix it and all. I have jewelry iv made waiting to be fired thats coe 96. I also have some scrap of 90 that I plan on making jewelry out of as well. Can I fire the two sets at the same time? im not mixing the 90-96 together im just going to fire the two separate sets on the same shelf at the same time. what firing schedule should I use? I mainly ask regarding the annealing time. bullseye and spectrum have different recommend annealing times so im a little hesitant to fire them both together. To be honest I havent really worked with bullseye to much. only about 3 times. I received some scraps from a friend and dont want them to just sit around.
Brad Walker
Site Admin
Posts: 1539
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Fusiing different coe glass in the same firing

Post by Brad Walker »

Yes, you can fire them in the same kiln.

Either annealing temperature will work. Given that that's what you're used to, I would use Spectrum's 950, but BE's 900 would be ok, as would the 960 BE used to recommend.