never fired a piece this large before, need some advice as to schedule for firing.
thanks
schedule for 50X25 piece, 6 mm thick
Moderators: Brad Walker, Tony Smith
schedule for 50X25 piece, 6 mm thick
Carol Ann
Re: schedule for 50X25 piece, 6 mm thick
http://www.warmglass.org/books/books/126-fsgCarol Ann wrote:never fired a piece this large before, need some advice as to schedule for firing.
thanks
Jerry
Re: schedule for 50X25 piece, 6 mm thick
thank you Jerry i will look into the book you suggested.