I am planning on doing a mesh melt and would like a little advice. I built a 15 in by 15 in by 4 1/2 box made of vermiculite and stainless steel screws. I have a stainless steel wire mesh for the top of the box. I also placed some screws on top of the box to hold the wire mesh in place. I prepped my kiln shelf with 5 layers of kiln wash. I plan on cutting 1/32 fiber blanket to line the box and come between the box and the glass. I have a couple questions 1) how much glass will I need to for the mesh melt (6mm thick) 2) I am looking for a suggested program (Jen-Ken AF3P 24E/15) Any suggestions would be greatly appreciated. Thank you!
Blair
Posts: 11
Joined: Wed Dec 05, 2007 12:24 am

Re: Mesh Melt

Post by Blair »

I forgot to a one detail. I am using bullseye 90 glass for the project. :)
Peter McCarthy
Posts: 19
Joined: Wed Feb 22, 2006 10:48 am
Location: Cambridge, MA

Re: Mesh Melt

Post by Peter McCarthy »

On fusedglass.org, there's a pot-drop volume calculator and schedule:
http://www.fusedglass.org/tools/pot_drop_calculator
http://www.fusedglass.org/downloads/sch ... hedule.pdf

And Steve Immerman's pot drop tutorial has a recommended schedule:
http://www.clearwaterglass.com/Tutorial ... ePour.html
The Hobbyist
Posts: 309
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: Mesh Melt

Post by The Hobbyist »

If you put the screws into the top edge of the vermiculite and don't bend the SS mesh over then I would expect the weight under heat to pull/rip the screws out of the vermiculite. It may all fall into the middle.

Jim

ps. Here's how I set it up:
Attachments
Dsc00068a.jpg
Dsc00065b.jpg
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
Blair
Posts: 11
Joined: Wed Dec 05, 2007 12:24 am

Re: Mesh Melt

Post by Blair »

Thank you for your advice. I appreciate the help! I have been putting off the project because I have been a little nervous about it. My project is a square piece so I will add a little more glass. I did use the pot melt calculator. Thanks, Blair