Glass turning silvery grey
Moderators: Brad Walker, Tony Smith
Glass turning silvery grey
So...what causes glass to turn silver grey? I have been having this happen with white and yellow glass lately, at all sorts of firing temps. It almost has a fumed look. Firings have included all sorts of other colors.
"Every artist was first an amateur."
--Ralph Waldo Emerson
--Ralph Waldo Emerson
Re: Glass turning silvery grey
Is it irid glass? What are you firing with it?
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Re: Glass turning silvery grey
just standard BE white. Not sure what you mean by what I'm firing it with. On kilnwash, mixed color loads. Nothing that I know of that should fume.
"Every artist was first an amateur."
--Ralph Waldo Emerson
--Ralph Waldo Emerson
-
- Posts: 186
- Joined: Fri Oct 31, 2008 9:26 am
- Location: Newtown, Sydney, Australia.
Re: Glass turning silvery grey
Does the silver grey look metallic?
Peter Angel
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
-
- Posts: 94
- Joined: Mon Nov 06, 2006 11:13 pm
- Location: Hillsboro, OR
- Contact:
Re: Glass turning silvery grey
Have you fired anything else in the kiln or on the shelf you are using other than BE glass? Like, clay, metal, or other types of glass?
Mike
Mike
It's said that inside each of us is an artist trying to get out. Well mine got out... and I haven't seen him since.
-
- Site Admin
- Posts: 1531
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Glass turning silvery grey
That kind of glass won't turn silvery grey without some sort of contamination in the kiln. Have you fired anything unusual in the firings prior to having the trouble? Fired anything other than just glass? Changed the kiln wash/shelf paper/kiln shelf/whatever? Used enamels/paints/inclusions/metals/whatever?
If you can, try a piece of the same glass in another kiln to see if the problem happens again. (Preferably someone else's kiln in another location.)
If you can, try a piece of the same glass in another kiln to see if the problem happens again. (Preferably someone else's kiln in another location.)
-
- Posts: 186
- Joined: Tue Dec 29, 2009 7:13 pm
- Location: Nahant Massachusetts
- Contact:
Re: Glass turning silvery grey
I am wondering the same thing, did you fire silver or metal clay in the kiln.
Bob
Bob
Re: Glass turning silvery grey
Previously fired silver stain?