Glass turning silvery grey

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Cheryl
Posts: 239
Joined: Sun Mar 09, 2003 7:56 pm
Location: Tallahassee FL
Contact:

Glass turning silvery grey

Post by Cheryl »

So...what causes glass to turn silver grey? I have been having this happen with white and yellow glass lately, at all sorts of firing temps. It almost has a fumed look. Firings have included all sorts of other colors.
"Every artist was first an amateur."

--Ralph Waldo Emerson
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Glass turning silvery grey

Post by Morganica »

Is it irid glass? What are you firing with it?
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Cheryl
Posts: 239
Joined: Sun Mar 09, 2003 7:56 pm
Location: Tallahassee FL
Contact:

Re: Glass turning silvery grey

Post by Cheryl »

just standard BE white. Not sure what you mean by what I'm firing it with. On kilnwash, mixed color loads. Nothing that I know of that should fume.
"Every artist was first an amateur."

--Ralph Waldo Emerson
Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: Glass turning silvery grey

Post by Peter Angel »

Does the silver grey look metallic?
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Mike Jordan
Posts: 94
Joined: Mon Nov 06, 2006 11:13 pm
Location: Hillsboro, OR
Contact:

Re: Glass turning silvery grey

Post by Mike Jordan »

Have you fired anything else in the kiln or on the shelf you are using other than BE glass? Like, clay, metal, or other types of glass?

Mike
It's said that inside each of us is an artist trying to get out. Well mine got out... and I haven't seen him since.
Brad Walker
Site Admin
Posts: 1540
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Glass turning silvery grey

Post by Brad Walker »

That kind of glass won't turn silvery grey without some sort of contamination in the kiln. Have you fired anything unusual in the firings prior to having the trouble? Fired anything other than just glass? Changed the kiln wash/shelf paper/kiln shelf/whatever? Used enamels/paints/inclusions/metals/whatever?

If you can, try a piece of the same glass in another kiln to see if the problem happens again. (Preferably someone else's kiln in another location.)
bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: Glass turning silvery grey

Post by bob proulx »

I am wondering the same thing, did you fire silver or metal clay in the kiln.
Bob
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Glass turning silvery grey

Post by Buttercup »

Previously fired silver stain?
Post Reply