Mounting Glass in a Shadow Box, Etc.

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
LDGlass
Posts: 22
Joined: Sun Mar 23, 2003 2:54 pm
Location: Milwaukee, WI
Contact:

Mounting Glass in a Shadow Box, Etc.

Post by LDGlass »

I was wondering the best way to attach glass to the back of a shadow box or a board or otherwise. I've seen fused glass in shadow boxes. This weekend I saw a fused glass panel maybe 8" x 14" mounted to what looked like a canvas in a frame.
Do you glue it somehow? A small piece I can image gluing to the inside of a shadow box but not sure about something large how to attach it. The one I saw this weekend looked really nice. I'd to do the same in the future for wall pieces.
Lauri Levanto
Posts: 270
Joined: Tue Mar 11, 2003 7:33 am
Location: Halikko, Finland

Re: Mounting Glass in a Shadow Box, Etc.

Post by Lauri Levanto »

Excuse my poor English. What is a shadow box?
-lauri
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Mounting Glass in a Shadow Box, Etc.

Post by DonMcClennen »

GE Silicone #2 is probably one of the best adhesives for fastening glass to many surfaces. I've used it for years both interior and exterior applications. NEVER had any failures. Some outside applications have stood hot summers, freezing winters, for 10 years and counting. (always use fresh product)
"The Glassman"
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Mounting Glass in a Shadow Box, Etc.

Post by Kevin Midgley »

LDGlass
Posts: 22
Joined: Sun Mar 23, 2003 2:54 pm
Location: Milwaukee, WI
Contact:

Re: Mounting Glass in a Shadow Box, Etc.

Post by LDGlass »

Thanks Don! That is what I will use. =D>
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: Mounting Glass in a Shadow Box, Etc.

Post by charlie »

and ace hardware has one that is crystal clear, but it's not GE and costs a bit more. GE doesn't sell a clear one in big box stores. you'd need this if the glass is translucent to any degree.
Redfisher
Posts: 20
Joined: Sat Feb 26, 2005 12:03 pm
Location: St Augustine, FL

Re: Mounting Glass in a Shadow Box, Etc.

Post by Redfisher »

My framer uses GE silicone and swears by it!
Terri
<'{{{{><
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Mounting Glass in a Shadow Box, Etc.

Post by Kevin Midgley »

beware some sealants that are "water" clear do not have the adhesive strength you may require as they are made to be a sealant rather than a glue.
I suspect it is like epoxy or concrete if you have a matrix of materials the strength is greater and clear sealants don't have that visible matrix.
Check the specifications carefully before choosing one.
I had this great idea and then.... #-o #-o #-o
Pipwren
Posts: 15
Joined: Sat Feb 15, 2014 10:22 am

Re: Mounting Glass in a Shadow Box, Etc.

Post by Pipwren »

I like the idea of shadow boxes too but think it would be more interesting to use a dark opaque around the perimeter of your work (making it look like a boxed frame) and imbed the work in clear. How cool would that look (much heavier to hang though)!
Post Reply