super easy question about priming a mold
Moderator: Tony Smith
-
lorimendenhall
- Posts: 91
- Joined: Wed Apr 10, 2013 8:54 pm
- Location: Orange County, CA
- Contact:
super easy question about priming a mold
dumb question but I've heard differing info... how many uses can you get out of a ceramic mold primed with Hotline Primo Primer? thanks!
Re: super easy question about priming a mold
It depends upon the temperature your slumping at, the shape of the mould and how well you protect the mould surface from damage while not in use. A well cared for, kiln-washed mould can handle many firings. There's no absolute number. Just inspect the surface for imperfections before each use and fire at the lowest temperature that gets the job done.
Sharol
Sharol
-
lorimendenhall
- Posts: 91
- Joined: Wed Apr 10, 2013 8:54 pm
- Location: Orange County, CA
- Contact:
Re: super easy question about priming a mold
thanks for your reply. I've been doing a few per coating so I guess I'll just keep doing that for now.
Re: super easy question about priming a mold
You should be able to get many firings from a good coating, especially with the shallower moulds.
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: super easy question about priming a mold
Primo is supposedly one-time use. If I valued the mold or the piece, I don't think I would push it, especially if going to fusing temps (which is often when you use Primo).lorimendenhall wrote:dumb question but I've heard differing info... how many uses can you get out of a ceramic mold primed with Hotline Primo Primer? thanks!
2 cents,
Dana W.