Post by Vonon »

I want to make a couple of small "coral" bowls. The tutorial I found used stainless bowls for shaping. Could I use my ball molds and slump or is there something about the spidery construction of these that wants to drape instead of slump? Of course these are for gifts that I need next week.
Vonon
Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: coral bowls

Post by Stephen Richard »

Both are possible. Different effect
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
Vonon
Posts: 195
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: coral bowls

Post by Vonon »

Thanks Stephen. I appreciate the reply. :)