firing a new mold
Moderator: Tony Smith
-
Paul Schulz
- Posts: 49
- Joined: Mon Apr 01, 2013 10:02 pm
- Location: Christchurch New Zealand
firing a new mold
hi guys i have some new ceramics mold up to 340 mm wide that i need to pre fire, but not sure about the firing rate and time . one program says a rate of 50c per hour to 800c ,,that's 16 hours ,,is this right ?? many thanks paul
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: firing a new mold
need more info. are you firing green ceramics? if not i see no need to prefire. just kilnwash and use. r.
artist, owner of wanchese art studio, marine finisher
-
lorimendenhall
- Posts: 91
- Joined: Wed Apr 10, 2013 8:54 pm
- Location: Orange County, CA
- Contact:
Re: firing a new mold
I've never pre-fired a mold BUT I just got a new one and the instructions say:
"pre-firing is recommended for molds larger than 30cm. this process strengthens the inner structures and makes the mold less susceptible to thermal shock." the directions are to go like you say below, 50 degrees C (122F) to 800 degrees C (1472F). no hold. let cool down at room temp. yes, that sounds like it would 16 hours to get to the temp but then it would take quite a few hours to cool back down to room temp.
"pre-firing is recommended for molds larger than 30cm. this process strengthens the inner structures and makes the mold less susceptible to thermal shock." the directions are to go like you say below, 50 degrees C (122F) to 800 degrees C (1472F). no hold. let cool down at room temp. yes, that sounds like it would 16 hours to get to the temp but then it would take quite a few hours to cool back down to room temp.
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: firing a new mold
What manufacturer recommends That? It makes no sense to me. R.
artist, owner of wanchese art studio, marine finisher
-
lorimendenhall
- Posts: 91
- Joined: Wed Apr 10, 2013 8:54 pm
- Location: Orange County, CA
- Contact:
Re: firing a new mold
this mold is manufactured by Creative Ceramics and I think it was a Bullseye branded item.
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: firing a new mold
huh. if the mold has been bisque fired. (those have) then it has been fired to above 1472. i can see no reason why doing like they said would do anything to the ceramic 'interior structures' or whatever. i just see no science behind that statement. cynthia m, you got a clue i am missing? r.
artist, owner of wanchese art studio, marine finisher
-
Glass Fever
- Posts: 29
- Joined: Sat Aug 04, 2007 11:08 pm
- Location: Chicago Suburbs
- Contact:
Re: firing a new mold
As a sometimes potter I agree with Rosanna. Firing an already bisqued mold to basically bisque temperature will do nothing to the internal structure. I have never prefired any of my Bullseye or other purchased molds.rosanna gusler wrote:huh. if the mold has been bisque fired. (those have) then it has been fired to above 1472. i can see no reason why doing like they said would do anything to the ceramic 'interior structures' or whatever. i just see no science behind that statement. cynthia m, you got a clue i am missing? r.
-
Paul Schulz
- Posts: 49
- Joined: Mon Apr 01, 2013 10:02 pm
- Location: Christchurch New Zealand
Re: firing a new mold
mmmm seems i have opened Pandora's box ,,the moulds are from creative ceramics and 15 " round or across. the instructions say to pre fire at a rate of 50c per hour to 800c ,time 960 minutes ,,the trouble with this program is that my kiln controller will not handle that as it is just too slow,,,,,,so to pre fire or not to pre fire
Re: firing a new mold
Not. I never have and had a lot of those molds.
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: firing a new mold
Makes you wonder what they are firing these slip cast molds to on their firing. There should be no need to fire it again. We bisque our thrown molds to 1900 and they last forever but they are a different clay body.
I would not prefire.
I would not prefire.
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com