Hi,
We are doing some pattern bars. We have slices about 1"x2" (sort of domino size). If we want to have them all in a row down the center of a platter, do you recommend us to first fuse the sliced pieces into a solid piece and then add the rest of the platter glass around it, or do you tend to put pattern slices in the middle of the platter, build rest of platter around it and then doing your full fuse all as one overall piece? Just didn't know if we should do this in two steps or one. Any comments are appreciated.
Thanks
Cherie
Pattern Bars help
Moderators: Brad Walker, Tony Smith
-
Cherie Knopf
- Posts: 14
- Joined: Tue Apr 23, 2013 8:37 pm
- Location: Morgan Hill, California
- Contact:
Re: Pattern Bars help
One step, dam it.