Belt Sander or Lap Wheel

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Cherie Knopf
Posts: 14
Joined: Tue Apr 23, 2013 8:37 pm
Location: Morgan Hill, California
Contact:

Belt Sander or Lap Wheel

Post by Cherie Knopf »

Hi, we have a small fused glass business and want to keep expanding our tools for the studio. I was curious, of your thoughts on tools. We have a wet saw and grinder, and ringsaw, but are thinking about getting either a lapwheel sander or a sanding belt sander to do more of the coldworking/finishing. For those of you that do a lot of cold working on fused items (usually plates, small dishes, jewelry - would you suggest our next purchase should be the lapwheel or a belt sander. What do most folks doing fused glass tend to prefer? We have a large non-profit studio where we can go to do some of this coldworking, but wanting to get more at home so we don't have to drive in. Any suggestions are appreciated.

Thanks
Cherie
jim burchett
Posts: 254
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: Belt Sander or Lap Wheel

Post by jim burchett »

Sander first then lap wheel...the bigger the better
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Belt Sander or Lap Wheel

Post by Morganica »

I agree, wet belt sander first, lapwheel second. The belt sander can be made to do flat surfaces (although it's not ideal) and straight edges, but it's tough to get a lap wheel to cover contours the way a belt sander can.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Marty
Posts: 862
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Belt Sander or Lap Wheel

Post by Marty »

what jim, cynthia and jim said
but
get bigger machines than you think you need.
In a year or so you will curse the benchtop sander and the 12" grinder.
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Belt Sander or Lap Wheel

Post by jim simmons »

I made an assumption, and we all know that assumptions are the mother of all screw ups :>)

I assumed that she would get the biggest one that she could afford.
The other Jim
misteroldhouse
Posts: 10
Joined: Tue Dec 04, 2007 1:02 am
Location: Dallas, Texas
Contact:

Re: Belt Sander or Lap Wheel

Post by misteroldhouse »

I agree with all, First the WBS, than a diamond lap.

In my experience, diamonds cut faster & deeper; one often has to use the WBS with t's silicon carbide wet belts in order to remove those fine diamond-produced scratches!

Larry
Larry Pile
Artist
Kessler Craftsman
Dallas, Tx
www.kesslercraftsman.com
Post Reply