With some other aerosol sprays (such as paint) you have to hold the can upside down and spray until only air comes out after you have used it.
Do you have to clear the tube after spraying MR-97?
Mary
			
			
									
						
										
						MR-97 mold release spray
Moderators: Brad Walker, Tony Smith
- 
				JestersBaubles
 - Posts: 705
 - Joined: Fri Feb 25, 2011 12:01 am
 - Location: North Logan, UT
 - Contact:
 
Re: MR-97 mold release spray
I never have....
Just my 2 cents worth of experience.
Dana W.
			
			
									
						
										
						Just my 2 cents worth of experience.
Dana W.
- 
				Laurie Spray
 - Posts: 321
 - Joined: Sat Dec 17, 2005 10:32 pm
 - Location: SANTA CRUZ, CALIFORNIA
 - Contact:
 
Re: MR-97 mold release spray
No.....just shake it well!
			
			
									
						
							Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
			
						New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
- 
				S.TImmerman
 - Posts: 235
 - Joined: Wed Nov 25, 2009 9:23 am
 - Location: San Diego ,Ca
 
Re: MR-97 mold release spray
Is it true , once you use mr-97 you can never go back to kiln wash?  Or is to the other way around?  One you use kiln wash you can't use MR-97 .. I was airbrushing kiln was and was told I could never use mr 97. 
Thank you
			
			
									
						
										
						Thank you
- 
				S.TImmerman
 - Posts: 235
 - Joined: Wed Nov 25, 2009 9:23 am
 - Location: San Diego ,Ca
 
Re: MR-97 mold release spray
Is it true , once you use mr-97 you can never go back to kiln wash?  Or is to the other way around?  One you use kiln wash you can't use MR-97 .. I was airbrushing kiln was and was told I could never use mr 97. 
Thank you
			
			
									
						
										
						Thank you
- 
				Laurie Spray
 - Posts: 321
 - Joined: Sat Dec 17, 2005 10:32 pm
 - Location: SANTA CRUZ, CALIFORNIA
 - Contact:
 
Re: MR-97 mold release spray
mr97 seals the clay molds in a way that repels regular kiln wash.  Since we are now a distributor of MR97 I have been doing further testing.  I have found that a light sanding is all that is needed if you want to switch.  That being said.....if you are using it on texture molds or casting molds you will not want to sand as you will lose some texture of course.  After we had used primo primer for years on texture molds I have found that with Mr97 the glass leaves less needling and releases clean and perfect and you get more texture.......You do need to brush the mold with a stiff brush between firings and just give it a "wisp" of a spray for the next  firing.  Love this spray!
			
			
									
						
							Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
			
						New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com