I am so satisfied that at the end it worked for me...........
This piece was fired twice in vain, the upper part [which was covered with fiber blanket] did not get enough heat and simpley broke.
I decided to fire it without the blanket, the way i learnt, and it came out quite nice.
Only there was a lot of devit on the edges. So used diluted spray A, used for the forming the schedule which is used by Moje, and rises as high as 750 Celsius.
The piece is formed, clean, no devit, and no signs of the explosion [ I have photos of this]
It is not EXACTLY what I was aiming to, but it is not a big compromise on my side. You can read about my dilemmas at the other forum which deals with firing etc.
I hope you like it - - -
Havi
a new piece I recently made
Moderator: Brad Walker
a new piece I recently made
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: a new piece I recently made
I think it's lovely. Good job!
Dana W.
Dana W.
-
Tammy Macdonald
- Posts: 15
- Joined: Tue Jun 18, 2013 1:45 pm
- Location: Texas
Re: a new piece I recently made
Havi,
I really like it! Quite lovely.
TAM
I really like it! Quite lovely.
TAM
-
bob proulx
- Posts: 186
- Joined: Tue Dec 29, 2009 7:13 pm
- Location: Nahant Massachusetts
- Contact:
Re: a new piece I recently made
It looks great Havi, sometimes the glass tells us what it wants to do.
Bob
Bob
-
Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: a new piece I recently made
lovely Havi,
Barry
Barry
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns