I have been testing Super Spray A for my bottle devit issues (I usually use Borax concoction with fair success).
I brush on Super Spray with a foam brush, then fire to 1430. The gloss looks good, but the bottles have brush streaks in the glass after firing.
Anyone have suggestions to eliminate the streaks?
Super Spray Streaking
Moderator: Tony Smith
Re: Super Spray Streaking
Go to Michael's or a craft store or art store and get a Badger air brush kit. Makes it a lot easier to use and no streaks. Helps to have a 40% off coupon for Michael s too.
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: Super Spray Streaking
Spray for sure!
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Re: Super Spray Streaking
Thanks for the tip. I bought a Badger 250-2 with a compressed air can to try (whole setup cost me ~$30 with coupon from Michaels.).
Results were much better.
I Just need a bit more practice to get more proficient with using the airbrush.
Results were much better.
I Just need a bit more practice to get more proficient with using the airbrush.
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Super Spray Streaking
And make sure you're shaking the container frequently. Using a brush means you're probably picking up more of the glass in the bottom of your container.