copper as a mold
Moderators: Brad Walker, Tony Smith
-
Karyn Cott
- Posts: 13
- Joined: Wed Sep 28, 2005 4:19 am
- Location: Poulsbo, WA
copper as a mold
I have a copper "jello" mold that states it is solid copper. Can I use this as a casting mold?
Karyn
"It is one of the blessings of old friends that you can afford to be stupid with them."
Ralph Waldo Emerson
"It is one of the blessings of old friends that you can afford to be stupid with them."
Ralph Waldo Emerson
Re: copper as a mold
Nope.
-
Karyn Cott
- Posts: 13
- Joined: Wed Sep 28, 2005 4:19 am
- Location: Poulsbo, WA
Re: copper as a mold
Thanks for the confirmation Brock.
Karyn
"It is one of the blessings of old friends that you can afford to be stupid with them."
Ralph Waldo Emerson
"It is one of the blessings of old friends that you can afford to be stupid with them."
Ralph Waldo Emerson