How to Make Rays of Sunlight?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Linda Gilpin
Posts: 12
Joined: Fri Oct 28, 2005 8:47 am
Location: Duncanville, TX

How to Make Rays of Sunlight?

Post by Linda Gilpin »

Any idea how you get those gorgeous rays of sunlight going through a piece? I assumed they were made with powders. I've seen some tree scenes lately with beautiful sun rays that aboslutely make the piece! Any thoughts or suggestions?
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: How to Make Rays of Sunlight?

Post by Kevin Midgley »

Tried putting your glass piece in sunlight.........?
Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: How to Make Rays of Sunlight?

Post by Laurie Spray »

Layers with powders......prefire each layer flat
then fuse together
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: How to Make Rays of Sunlight?

Post by Valerie Adams »

It seems to me the 'rays' I've seen in many landscapes are actually absence of color, with the powder/frit illustration being done on transparent glass.
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Re: How to Make Rays of Sunlight?

Post by Don Burt »

Silver stain, sometimes.
Pat Donaldson
Posts: 25
Joined: Fri Aug 10, 2007 9:45 am

Re: How to Make Rays of Sunlight?

Post by Pat Donaldson »

I posted one of my landscapes in the photo section. I get the rays of moonlight or sunlight by fusing several times with a light color that fits with the rest of the scene. Hope this helps!@

Pat