Anyone come up with a good base/mix of frit to come up with a realistic tree trunk color? I have tried grey with various brown and or black medium 90 coe frits and a mix of grey/black and also brown frit. I was thinking maybe I should wash some fine powdered black frit across some grey base. This will be for areas of glass where the tree trunk will be quite wide (200mm wide by 1.5meters) hence the need for the color to look realistic. Some of the streaky bullseye has the looks I want but I need to be able to create a continuous pattern across the whole trunk. The trunk itself will probably be opaque.
carol carson
Posts: 58
Joined: Sat Jul 30, 2005 6:25 pm
Location: Portland OR
Contact:

Re: Tree trunk/bark color

Post by carol carson »

Woodland Brown works well.
Pipwren
Posts: 15
Joined: Sat Feb 15, 2014 10:22 am

Re: Tree trunk/bark color

Post by Pipwren »

Thank you. Will try that. Have tried a base of just grey running uneven cuts along the glass so there are a lot of pieces. Then put them back together with a little gap between pieces and sprinkling black frit in the gaps (letting some fall on the grey glass itself). Then firing that. Looks pretty good but needs a bit more tweaking. Will now try your suggestion and some different colour frits. Mainly looking at gum tree bark which is more grey than brown. Thank you
Lynn Perry
Posts: 129
Joined: Sun Jun 08, 2003 5:27 pm
Location: East Tennessee

Re: Tree trunk/bark color

Post by Lynn Perry »

Thought you might get some ideas from the formulae used to create these stone effects.

http://www.fusedglass.org/learn/project ... faux_stone
Lynn Perry
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Tree trunk/bark color

Post by DonMcClennen »

I find paintings much more interesting when the "Artists" use red, blues. purples etc. to represent tree images!
"The Glassman"
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Tree trunk/bark color

Post by Brock »

So . . . you must love Andre Derain . . .
Pipwren
Posts: 15
Joined: Sat Feb 15, 2014 10:22 am

Re: Tree trunk/bark color

Post by Pipwren »

Agreed about using red blue and purple for tree trunks to make it more interesting. Was actually reading an art site ( http://willkempartschool.com/how-to-ins ... -painting/) That explains why we should think about darker colours to give depth.
As the trees will be in the foreground though I am not sure will work.
Brad Walker
Site Admin
Posts: 1540
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Tree trunk/bark color

Post by Brad Walker »

Brock wrote:So . . . you must love Andre Derain . . .
I was thinking Wolf Kahn.

Sometime his trees are in the foreground, too.
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Tree trunk/bark color

Post by DonMcClennen »

Brad Walker wrote:
Brock wrote:So . . . you must love Andre Derain . . .
I was thinking Wolf Kahn.

Sometime his trees are in the foreground, too.
Love Wolf Kahn =D> ... So refreshing from the standard landscape painters.
"The Glassman"
Post Reply