Latest Blanket Piece

Want to share a photo of your work? Or get feedback on a new piece? Post it here. (Note: items in this forum are deleted periodically, generally after several months.)

Moderator: Brad Walker

Post Reply
Yardic Glassworks
Posts: 80
Joined: Sat Mar 06, 2010 9:29 am

Latest Blanket Piece

Post by Yardic Glassworks »

Fresh from the oven...
Attachments
Blanket Web2.jpg
Blanket Web.jpg
Tim Yardic
Yardic Glassworks
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Latest Blanket Piece

Post by twin vision glass »

Beautiful and stunning and well, just wonderful. Les
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Latest Blanket Piece

Post by JestersBaubles »

Your blankets are amazing. Thank you for sharing them

Dana W.
Vonon
Posts: 195
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: Latest Blanket Piece

Post by Vonon »

Stunning is the word! Just love the color selection on this one.
Vonon
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Latest Blanket Piece

Post by Buttercup »

Congratulations again, Tim, another beauty. Jen