silver and glass
Moderators: Brad Walker, Tony Smith
-
- Posts: 3
- Joined: Mon Mar 18, 2013 9:57 pm
silver and glass
Can you fire silver with glass?
-
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: silver and glass
Yes, but it does depend on the thickness of the silver and the glass it is fused with (reactivity)
I screen print silver slip all the time on to BE1401.
Difficult to cap.....yellows.
I screen print silver slip all the time on to BE1401.
Difficult to cap.....yellows.
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
-
- Posts: 91
- Joined: Wed Apr 10, 2013 8:54 pm
- Location: Orange County, CA
- Contact:
Re: silver and glass
if you use fine silver it will stay bright silver colored. if you use sterling silver it turns ugly. I embed fine silver hangers into pendants all the time.
-
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: silver and glass
Make sure to take into considerations the reactions due to the silver. You might want to look at a blog post I did on Bullseye reactive glass:
http://jestersbaubles.blogspot.com/2014 ... glass.html
Dana W.
http://jestersbaubles.blogspot.com/2014 ... glass.html
Dana W.