I'm looking for a silver enamel similar to Hanovia Gold, Thompson Gold, or Duncan Gold. in searching for the silver, I'm no longer finding the gold ones either. So, is there a silver liquid enamel? And, do I need to begin hoarding my remaining bottles of the above named gold ones?
There was a lot of conversation about the golds in the past, but I'm not finding them under search.
gold and silver enamels
Moderators: Brad Walker, Tony Smith
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: gold and silver enamels
There are platinum and palladium for the silver color. Hereaus is now the premier manufacturer of precious metal lustres. There are also Chinese knockoffs.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: gold and silver enamels
Unique Glass Colors makes a couple metallic paints that work fairly well and are very inexpensive. I'm hoarding my bottles of the real stuff!