I tried pot melting for the first time. I used a small terracotta pot and a recommended firing schedule. When it was done there was melted glass in the pot and a stream of glass connecting the bottom of the pot to the glass in the mold below. What caused this? I really need help. Thanks.
Re: Pot melt problem
I'm definitely not qualified to give advice but check this out:
http://www.warmglass.com/phpBB/viewtopi ... =2&t=39790
Have fun
Jen
http://www.warmglass.com/phpBB/viewtopi ... =2&t=39790
Have fun
Re: Pot melt problem
not hot enough for long enough.
Re: Pot melt problem
That's normal. You needed more heat and more time.
-
colettecoad
- Posts: 3
- Joined: Fri Oct 25, 2013 2:30 pm
Re: Pot melt problem
Thanks to all for the links and advice. I will try hotter and longer.
Re: Pot melt problem
Got a peep hole? One quick glance will tell you whether it's done or not.