What not to do
Moderators: Brad Walker, Tony Smith
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
What not to do
Oops, ramped a little too fast (and I knew better...) 
-
Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: What not to do
Don't give up on the piece Dana,
Need to find a useful function for it..
Maybe a downspout receptor, or a wall mounted mail holder.
Barry
Need to find a useful function for it..
Maybe a downspout receptor, or a wall mounted mail holder.
Barry
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: What not to do
Or whack it with a hammer and start all over
Dana W.
Dana W.
Re: What not to do
What a shame! Beautiful colors!
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: What not to do
Or trim it so you have a ring, fuse it to a double-layer of white or off-white, and put it back into the same mold for a unique two-toned piece.
Never give up!
Tony
Never give up!
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: What not to do
Yes, I've considered using the ring as a border to another piece. It would be easy to cut out -- it's half way thereTony Smith wrote:Or trim it so you have a ring, fuse it to a double-layer of white or off-white, and put it back into the same mold for a unique two-toned piece.
Never give up!
Tony
Dana