casting in pyramid mold

Use this forum for discussion on kiln casting, pate de verre, and related topics.

Moderator: Brad Walker

Post Reply
Bonnie Rubinstein
Posts: 239
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

casting in pyramid mold

Post by Bonnie Rubinstein »

first time casting- I am casting in a pyramid mold, about 3" high and 3" wide at base. Using system 96. Will use bits and pieces of glass. They do not have a schedule for a deep mold. I assume I will get lots of bubbles, and run the risk of breakage if it is not annealed properly.

Have anyone cast in this type of mold with 96, and can offer a schedule?
Thanks!
Bonnie Rubinstein
beninfl
Posts: 46
Joined: Sat Feb 08, 2014 8:54 pm

Re: casting in pyramid mold

Post by beninfl »

I'm curious too, I unpacked my Slympys Pyramid mold last night and gave it a spray of MR-97. It's a lot bigger than I thought it would be.
Bonnie Rubinstein
Posts: 239
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: casting in pyramid mold

Post by Bonnie Rubinstein »

I used primo primer on mine. did I need to use boron?

(FYI- I have a smaller pyramid as well, brand new , if you want to buy it.)

any schedules out there?
Bonnie Rubinstein
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: casting in pyramid mold

Post by DonMcClennen »

I've cast several... the size and number of your bubbles will change with the size of glass chunks you use... bigger chunks less bubbles.
Standard kilnwash coating works fine.
"The Glassman"
Bonnie Rubinstein
Posts: 239
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: casting in pyramid mold

Post by Bonnie Rubinstein »

Don, do you have a schedule? Do you use 90 or 96?
thanks
Bonnie Rubinstein
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: casting in pyramid mold

Post by JestersBaubles »

Here is the bullseye schedule. I found this by googling "pyramid mold firing schedule"

http://www.bullseyeglass.com/methods-id ... sting.html

Dana W.
Post Reply