M-97 versus Slide 1800

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
SusanHyatt
Posts: 16
Joined: Wed Feb 15, 2012 2:07 pm

M-97 versus Slide 1800

Post by SusanHyatt »

Hi All,

I am making now using M-97 for some molds. I have seen something called Slide Hi-Temp 1800. Can I use that on the same molds that I have been using M-97?
Thanks,
Susan
Brad Walker
Site Admin
Posts: 1537
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: M-97 versus Slide 1800

Post by Brad Walker »

You can use either. Most people say the M-97 is a little better quality. It's also more expensive.
Lori Schinelli
Posts: 19
Joined: Sun Nov 20, 2005 8:25 am
Location: Atlanta, Georgia

Re: M-97 versus Slide 1800

Post by Lori Schinelli »

Hi Brad. Im surprised to hear you had no trouble with the slide 1800. How high did you fire it? I broke several expensive color de verge molds by trying it instead of mr-97. Just curious
Lori
Brad Walker
Site Admin
Posts: 1537
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: M-97 versus Slide 1800

Post by Brad Walker »

Lori Schinelli wrote:Hi Brad. Im surprised to hear you had no trouble with the slide 1800. How high did you fire it? I broke several expensive color de verge molds by trying it instead of mr-97. Just curious
I only use the Slide on stainless molds, not on Colour de Verre molds. For those I use Primo Primer, which is what they used to recommend. Primo is less expensive than any of the boron nitride sprays.
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: M-97 versus Slide 1800

Post by JestersBaubles »

My personal experience is that every time I have used Slide on a stainless floral former, the inside of the glass has had milky/hazy spots where the glass touched the Slide. The one time I used it on a stainless drop mold, the glass stuck.

So... I think it sucks :mrgreen: . I will pay extra for the MR-97.

2 cents,

Dana W.
Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: M-97 versus Slide 1800

Post by Laurie Spray »

mR97 is not more expensive when you know where to buy it!!
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
suds
Posts: 34
Joined: Fri May 09, 2014 10:44 pm
Location: Sonoma County, CA

Re: M-97 versus Slide 1800

Post by suds »

Laurie Spray wrote:mR97 is not more expensive when you know where to buy it!!
OK, I'll bite. Where do you buy it?
I seem to go through an awful lot of it and would love a cheaper source.
Steve
Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: M-97 versus Slide 1800

Post by Laurie Spray »

Check our site;)
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
B.J.
Posts: 5
Joined: Wed Oct 11, 2006 12:55 pm
Location: Virginia

Re: M-97 versus Slide 1800

Post by B.J. »

It is still more expensive than Slide but I would not use Slide on my Colour de Verre molds. They do recommend MR-97 and if you shop around you can find some pretty good prices. Laurie requires a minimum purchase on her site to get the lower price. I do use Slide on my stainless steel molds with no problems.
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: M-97 versus Slide 1800

Post by Valerie Adams »

B.J. wrote:Laurie requires a minimum purchase on her site to get the lower price.
[edited to remove pricing information...]

I can vouch for how easy it is to spend on her site; her stainless shapes are the best, and if you've never used the bottomless molds, you're in for a treat.
Last edited by Valerie Adams on Tue May 26, 2015 1:33 pm, edited 1 time in total.
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: M-97 versus Slide 1800

Post by JestersBaubles »

Anywhere you buy, except a retail store, will have a minimum order.

I get my glass from D&L. Their price for MR-97 is only a few dollars more than Laurie's, but there's a $75 minimum order. So... if all you need are MR-97 and molds, I would talk with Ms. Spray :)

Dana W.