I have a source for a lot of plate glass that is o.25" X  11.5" X 29" and the lady would like to have some compensation for it.  Would anyone have any idea what a fair price I should give her would be?
BTW, this is NOT float.  I don't know if it is vertically drawn or if it has been polished. The only thing I know is that it does not have a "tin glow" when I put my lamp to it.
Thanks
Jim S
			
			
									
						
							plate glass cost question.
Moderators: Brad Walker, Tony Smith
- 
				jim simmons
 - Posts: 478
 - Joined: Sun Mar 09, 2003 10:37 pm
 - Location: Hillsboro Oregon
 - Contact:
 
- 
				Bert Weiss
 - Posts: 2339
 - Joined: Tue Mar 11, 2003 12:06 am
 - Location: Chatham NH
 - Contact:
 
Re: plate glass cost question.
Jimjim simmons wrote:I have a source for a lot of plate glass that is o.25" X 11.5" X 29" and the lady would like to have some compensation for it. Would anyone have any idea what a fair price I should give her would be?
BTW, this is NOT float. I don't know if it is vertically drawn or if it has been polished. The only thing I know is that it does not have a "tin glow" when I put my lamp to it.
Thanks
Jim S
It is probably polished plate. They used to double roll and polish 1/4" glass. I would offer her .30 - .50 per square foot unless there is some antique value to it. It is probably scratched. The good news is that if you enamel on it, you will fill the scratches and have a new glass surface.
I pay less that $1 per foot in case lots. Salvage glass should be cheap. I'd aim at the low number or lower.
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				jim simmons
 - Posts: 478
 - Joined: Sun Mar 09, 2003 10:37 pm
 - Location: Hillsboro Oregon
 - Contact:
 
Re: plate glass cost question.
Thanks, BertBert Weiss wrote:Jimjim simmons wrote:I have a source for a lot of plate glass that is o.25" X 11.5" X 29" and the lady would like to have some compensation for it. Would anyone have any idea what a fair price I should give her would be?
BTW, this is NOT float. I don't know if it is vertically drawn or if it has been polished. The only thing I know is that it does not have a "tin glow" when I put my lamp to it.
Thanks
Jim S
It is probably polished plate. They used to double roll and polish 1/4" glass. I would offer her .30 - .50 per square foot unless there is some antique value to it. It is probably scratched. The good news is that if you enamel on it, you will fill the scratches and have a new glass surface.
I pay less that $1 per foot in case lots. Salvage glass should be cheap. I'd aim at the low number or lower.
Jim