Does anyone re-use 1/8" fiber paper? I have been saving it for a few years with the thought of using it again. Can I use it dry? Or should I wet it to shape, then dry out before using? Anyone do this?
Cate
Re-using 1/8" fiber paper
Moderators: Brad Walker, Tony Smith
Re: Re-using 1/8" fiber paper
yes, but it's lost its stiffness. you could wet it with a sugar solution (7up), roll it out flat, and let it dry (or use a slab roller if you have access to a ceramic's shop).
i use wads of it as filler in bottle necks if i'm flattening a bunch for friends.
i use wads of it as filler in bottle necks if i'm flattening a bunch for friends.
Re: Re-using 1/8" fiber paper
Thanks, Charlie. I was actually going to mound it up and fuse something over it.
Cate
Cate
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Re-using 1/8" fiber paper
I am a big fan of Unifrax 1/4" blanket. I use the fibers from this over and over for many different kinds of molds. The fiber from papers is not very good for keeping it's shape. The blanket is great.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: Re-using 1/8" fiber paper
Thanks Bert. I don't know what type of stuff I have; It's not paper though. It is soft after firing and I thought I would turn a ceramic mold upside down and use this spent paper/blanket to cover the mold. I need this mold for the shape I need for my glass piece. I would like to get it as smooth as I can, so I wondered if I should use some kind of binder to make it easier to mold. I was going to spray it with kiln wash , too.
Cate
Cate
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Re-using 1/8" fiber paper
I get smoother by using very finely ground alumina hydrate, like JM Huber SB432. However you can't really get smooth when the mold is on contact with something solid. I know people struggle with this impossible task. My personal approach is: If I can't get rid of texture, make it interesting, and make it an integral part of my design. This works much better for me than, "almost smooth but not quite there". The alternative is to do drop molds and cut the top off.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: Re-using 1/8" fiber paper
Good idea about the texture. I was thinking I will never get it smooth. I'm going to try it and see what happens.
Thanks,
Cate
Thanks,
Cate
Re: Re-using 1/8" fiber paper
I sometimes use spent fiber in refractory molds, for reinforcement. Works very well, also tends to aerate the mold mix a bit.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Re: Re-using 1/8" fiber paper
I would really like to take a class in mold making. Haven't seen any available near me in a while.
Cate
Cate