Post by Joe Pfeifer »

Does anyone know if "Spinel" ramming refractory material would be useful as a component in making your own investment for lost wax casting, or for bead release, or for any other "glass" use?:
Al2O3 89%
SiO2 0.5%
MgO 10%

I have a whole bunch available...
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Refractory Materials

Post by Brad Walker »

What's it manufactured to be used for?
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: Refractory Materials

Post by rosanna gusler »

Ask on craftweb hot glass. They will know.
artist, owner of wanchese art studio, marine finisher
Joe Pfeifer
Posts: 24
Joined: Thu May 27, 2010 9:55 pm

Re: Refractory Materials

Post by Joe Pfeifer »

It is a dry ramming material manufactured specifically for use in the installation of pre-formed alumina crucibles and ladles for the steel industry.

http://www.engineeredceramics.com/produ ... erial.html
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Refractory Materials

Post by Brad Walker »

The folks at Craftweb would surely know more about the product than here. If nothing else, Pete has a lot of crucible knowledge.

http://talk.craftweb.com/forumdisplay.php?s=&forumid=4
Post Reply