I am wanting to attach fused glass tiles to stainless steel or aluminum after using a dremel tool on the metal. Any suggestions on what to use. Also, thinking about trying to put something behind the glass to add some depth. Also, looking for suggestions on what to put on the back so it can be hung.

Thanks.
Deb
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: Attaching glass to stainless steel

Post by charlie »

ge silicone 2. don't forget to let sit untouched for 24 hours as a minimum
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Attaching glass to stainless steel

Post by Brad Walker »

charlie wrote:ge silicone 2. don't forget to let sit untouched for 24 hours as a minimum
And be sure to use a fresh tube.
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Attaching glass to stainless steel

Post by Bert Weiss »

The depth thing comes when the glass is not in contact with the metal. So put the silicone around the perimeter making sure the glass does not touch the metal. Light will go through and bounce back.

Another good adhesive is VHB tape. VHB stands for very high bond. Letting it sit for up to 3 days will help develop strength.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Deb
Posts: 7
Joined: Sun Feb 22, 2004 11:12 pm

Re: Attaching glass to stainless steel

Post by Deb »

I am thinking of using plexiglass to attach fused glass to Aluminum. For the back, looking at different stand off systems. Any suggestions on what type might be good?