Tack fuse first?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Emily Will
Posts: 27
Joined: Fri Dec 14, 2012 1:08 am

Tack fuse first?

Post by Emily Will »

I'm trying to make a "tartan" bowl for a wedding present. After experimenting with colors,
I've cut red and greed transparent strips. I have two layers with the strip colors in different
positions, and the plan is to fuse them with one layer 90 degrees rotated to get the "weave"
look. There will be a few yellow stringers on top.

As I got ready to fuse the circle, I realized how many potentials for bubbles there are and
I wonder if the smarter way would be to tack fuse each layer separately and then orient them
and do a full fuse (with the stringers on top) before slumping.

Does that make sense? Any better approach?

Thanks,
Emily
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Tack fuse first?

Post by JestersBaubles »

You can do a "fake weave" by placing one strip horizontally, then the next strip vertically, then horizontally, then vertically... etc. I have done this a few times and you do not get bubbles if you are building in a single layer or on top of another layer. You would get bubbles if you tried to cap it.

Just keep in mind that your red and green will be black where they overlap. Since this is a tartan, maybe that is what you are planning.

Dana W.
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Tack fuse first?

Post by JestersBaubles »

This is the "fake weave". You'll notice that the last strip placed ends up not looking woven (the blue horizontal strip closest to the camera in this view).
Attachments
blueyellowweave.jpg
blueyellowweave.jpg (9.88 KiB) Viewed 10050 times
misteroldhouse
Posts: 10
Joined: Tue Dec 04, 2007 1:02 am
Location: Dallas, Texas
Contact:

Re: Tack fuse first?

Post by misteroldhouse »

It's not necessary to tack fuse everything if your only op intent is to avoid bubbles. After all. The tack fuse isn't a full fuse & so will leave the same bubble-causing spaces! Look up "bubble squeeze" firing schedules and try that, knowing that some bubbles are just unavoidable period! L~
Larry Pile
Artist
Kessler Craftsman
Dallas, Tx
www.kesslercraftsman.com
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Tack fuse first?

Post by JestersBaubles »

misteroldhouse wrote:It's not necessary to tack fuse everything if your only op intent is to avoid bubbles. After all. The tack fuse isn't a full fuse & so will leave the same bubble-causing spaces! Look up "bubble squeeze" firing schedules and try that, knowing that some bubbles are just unavoidable period! L~
You won't get bubbles in this design -- the open spaces are on top, with plenty of room for the air to escape (in fact, it would be difficult to *try* to trap bubbles if you are using relatively narrow strips, which you would do with weaving). The only way you would get bubbles is if you tried to cap it with clear or something.

Dana