Jewellery box.
Moderator: Brad Walker
Jewellery box.
Finally found the time to finish off something for a friend. The lid is made from thin strips of float laid into an open mould dug into a kiln brick. The body of box is a failed bubble block ground to shape and polished. Not keen on waste so was happy enough to put the hours in for someone who's been there for us. peace, haydo
Life is like a raft, so be like a rat!...Challenging being a captain type rat though, going down with each ship and all!!
Re: Jewellery box.
Wow, Haydo! Looks like a lot of coldworking on your part. I think your failure has turned into a huge success. Again, wow!
Jeanice
Re: Jewellery box.
It's just beautiful, Haydo. I am so impressed by your bubble blocks. The movement is visually very compelling. What a lovely and generous gift for your friend.
Sharol
Sharol
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Jewellery box.
I love that the heart is revealed as the box is opened. Beautiful work and a very special gift!
-
Pat Donaldson
- Posts: 25
- Joined: Fri Aug 10, 2007 9:45 am
Re: Jewellery box.
That is an intrigueing(sp?) piece. I'd love to figure out how to do that! It's really lovely!
Pat
pat@aslowfuse.com
Pat
pat@aslowfuse.com
Re: Jewellery box.
Lovely piece, Haydo, a very special gift. What are the dimensions? Jen
Re: Jewellery box.
Compliments are appreciated, thank you. Small kilns can do a lot in a studio. Won't try and revisit this too soon but am happy it's something that can be tweaked and played with down the track. To figure it out is just a matter of working out how to get a bubble to stay where it's wanted, journey is half the fun.
Jen, the block containment starts at between 85 to 90mm square, with a bit of heat up its bum this can change. Mad rush to finish this off before fly out to Nauru and have only now realised that I didn't engrave it as I was supposed to do. peace, haydo
Jen, the block containment starts at between 85 to 90mm square, with a bit of heat up its bum this can change. Mad rush to finish this off before fly out to Nauru and have only now realised that I didn't engrave it as I was supposed to do. peace, haydo
Life is like a raft, so be like a rat!...Challenging being a captain type rat though, going down with each ship and all!!
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: Jewellery box.
Very beautiful. I'd say that is more than a happy accident!
Dana
Dana
Re: Jewellery box.
Pay attention while you're on Nauru, don't get sucked in by the travel brochures for Cambodia! Jen
Re: Jewellery box.
I feel genuinely sad for any of the pawns in this game of "bring on police state" that have a real need to resettle in Australia. Cambodia could be a win win, and may allow to show how the world can move forward from all of this fear and hatred. Could become the perfect model. Now that would be some @#$%&*! artist to pull that one off.
For now the problem of terrible "terrorism" is paying for me to have studio time. At the moment I can't afford to be politically reactive, but my cause will always be the problem of discreet genocide in West Papua. Just need the balls to jump off of the thingamejig that rats run around on. peace, haydo
For now the problem of terrible "terrorism" is paying for me to have studio time. At the moment I can't afford to be politically reactive, but my cause will always be the problem of discreet genocide in West Papua. Just need the balls to jump off of the thingamejig that rats run around on. peace, haydo
Life is like a raft, so be like a rat!...Challenging being a captain type rat though, going down with each ship and all!!
Re: Jewellery box.
I like this piece
Looks very nice to me, I am sure your friend will enjoy it.
Havi
Looks very nice to me, I am sure your friend will enjoy it.
Havi
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com