After coming home from a show, I noticed a small scratch on top of my item.   Normally, I would put it back in the kiln and polish it but I have glued cabochons on the bottom with E6000.    Any suggestion on how to fix the scratch or how to loosen up E6000 between 2 pieces of glass?   Thanks.
Deb
			
			
									
						
										
						Scratch on final product
Moderators: Brad Walker, Tony Smith
- 
				Georgia Novak
 - Posts: 28
 - Joined: Wed Jun 04, 2003 2:54 am
 
Re: Scratch on final product
soak it in Acetone until loose.  Pour the Acetone in a container that you can put a lid on or it will evaporate before it separates the pieces.