Calculate weight

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Joe Wokovich
Posts: 32
Joined: Tue Sep 25, 2007 1:57 pm
Location: Florissant, MO (@ St. Louis, MO)

Calculate weight

Post by Joe Wokovich »

Need Info:
I have another order for an oversized vase. Dimn are 36”long x 8”wide x 6”deep.
That is going to hold about 1 cubic foot of planting mix.
Currently I’m hoping to make this out of 6 mm float and I’m trying to see if the 6mm glass is thick enough to hold this weight.

Any thoughts??
Thanks
“If you tell me, I will forget.
If you show me, I will remember.
If you let me do it, I will understand."

And then tomorrow I can start all over again
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Calculate weight

Post by Bert Weiss »

I'm a fan of 10mm glass.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Joe Wokovich
Posts: 32
Joined: Tue Sep 25, 2007 1:57 pm
Location: Florissant, MO (@ St. Louis, MO)

Re: Calculate weight

Post by Joe Wokovich »

Bert I was wondering about how much soil weight I can put in this and still be safe

I'm looking at potting soil adds now to see how much a cubic foot it weighs.
Thanks
“If you tell me, I will forget.
If you show me, I will remember.
If you let me do it, I will understand."

And then tomorrow I can start all over again
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: Calculate weight

Post by charlie »

it weighs lots more once you water it. you also need drainage out the bottom.
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Calculate weight

Post by Bert Weiss »

I don't know. 10mm is beefier than 6mm. 6mm might work.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Calculate weight

Post by Buttercup »

Can't answer your question, Joe, but I am curious. Are you slumping to achieve this shape or are you adhering pieces together with UV adhesive or something similar? Jen
Post Reply