T-Fal Forms

Post by Jerrwel »

I just found a T-Fal coated cooking utensil that would make a great slumping mold if safe. I read a generalized MSDS on T-Fal which did not address what happens in temperatures greater than 350F. While sandblasting the item is probably what I'll do to remove the coating, I do wonder about the consequence of firing T-Fal in a kiln. Anyone have any info?
Jerry
jim burchett
Posts: 255
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: T-Fal Forms

Post by jim burchett »

You can try it in your kiln and let us know....:)
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
suds
Posts: 34
Joined: Fri May 09, 2014 10:44 pm
Location: Sonoma County, CA

Re: T-Fal Forms

Post by suds »

The teflon will burn off in the kiln and the byproducts of decomposition are probably pretty nasty.
I would be very hesitant to put T-fal in a kiln for fear of contamination or element damage and I sure as hell wouldn't do it unless the kiln was outdoors or extremely well ventilated tot he outside world.

I think I'd sandblast all the teflon off if I really wanted to use it.
Steve
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: T-Fal Forms

Post by rosanna gusler »

yep toxic as hell to burn off. r.
artist, owner of wanchese art studio, marine finisher
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: T-Fal Forms

Post by Marty »

http://www.t-falusa.com/Consumer+servic ... 59FBCB4%7D

I didn't bother to find out what the metal is.

Don't.
suds
Posts: 34
Joined: Fri May 09, 2014 10:44 pm
Location: Sonoma County, CA

Re: T-Fal Forms

Post by suds »

Marty wrote:http://www.t-falusa.com/Consumer+servic ... 59FBCB4%7D

I didn't bother to find out what the metal is.

Don't.
Heh. It's aluminum.
Steve