Sealing Agents
Moderators: Brad Walker, Tony Smith
- 
				Yardic Glassworks
 - Posts: 80
 - Joined: Sat Mar 06, 2010 9:29 am
 
Sealing Agents
I am in the process of a fairly comprehensive testing of several dozen different sealers for the use on sandblasted objects.  If anyone has a favorite that they are willing to share, I would love to include it in the testing process.  I will be happy to share the results when complete.  Thanks, Tim
			
			
									
						
							Tim Yardic
Yardic Glassworks
			
						Yardic Glassworks
Re: Sealing Agents
temporary:
Armorall
Mineral oil (warmed?)
Pledge
WD40
Teak Oil
more permanent:
any clear non-yellowing polyurethane
			
			
									
						
										
						Armorall
Mineral oil (warmed?)
Pledge
WD40
Teak Oil
more permanent:
any clear non-yellowing polyurethane
- 
				Suzanne Chudnoff
 - Posts: 10
 - Joined: Fri Mar 22, 2013 4:52 pm
 
Re: Sealing Agents
My favorite is still Liquid Luster that I buy from HIS.  I'm not sure what it's made of, but you don't have to use very much of it.  I've tried some other products, but they didn't give the same results.  What I like about it is that you can put on a very thin coat, and protect it from finger prints and keep a very matte surface.  Or if you put on subsequent coats, you can gloss it back up a little or a lot.  I still prefer prefer putting the piece back in the kiln to take it to a specific non gloss temperature, but when that's not possible, I'll use the Liquid Luster.
Suzanne
			
			
									
						
										
						Suzanne
- 
				Bob
 - Posts: 215
 - Joined: Mon Mar 10, 2003 1:01 pm
 - Location: Salt Spring Island, British Columbia
 - Contact:
 
Re: Sealing Agents
Hi Tim,
In addition to Marty's list I have heard of Danish Tung Oil, beeswax, the stuff used to sheet water off glass in showers.
I have often wondered about the sealer that is used for stone tile flooring.
I asked Mark Bollick at HISglassworks about sealers and he said that tung oil will yellow with time and becomes brittle so it may flake off the glass.
Like Suzanne, I like Liquid Lustre but it only has a 1 year shelf life.
Cheers,
Bob
			
			
									
						
										
						In addition to Marty's list I have heard of Danish Tung Oil, beeswax, the stuff used to sheet water off glass in showers.
I have often wondered about the sealer that is used for stone tile flooring.
I asked Mark Bollick at HISglassworks about sealers and he said that tung oil will yellow with time and becomes brittle so it may flake off the glass.
Like Suzanne, I like Liquid Lustre but it only has a 1 year shelf life.
Cheers,
Bob
- 
				rosanna gusler
 - Posts: 730
 - Joined: Mon Mar 10, 2003 2:22 pm
 - Location: wanchese north carolina
 - Contact:
 
Re: Sealing Agents
That's a great name.  Calls to mind another era, before focus groups.
Like Rosanna's Glassorama?
			
			
									
						
										
						Like Rosanna's Glassorama?
- 
				rosanna gusler
 - Posts: 730
 - Joined: Mon Mar 10, 2003 2:22 pm
 - Location: wanchese north carolina
 - Contact:
 
Re: Sealing Agents
I was wrong. Invisable shield. Our local grocery is the foodorama. Their slogan is "you can't beat our meat ".Marty wrote:That's a great name. Calls to mind another era, before focus groups.
Like Rosanna's Glassorama?
artist, owner of wanchese art studio, marine finisher
			
						- 
				JestersBaubles
 - Posts: 705
 - Joined: Fri Feb 25, 2011 12:01 am
 - Location: North Logan, UT
 - Contact:
 
Re: Sealing Agents
LOL! We have a plumber in town who had the slogan "Don't sleep with a drip" painted on his van. The very funny thing is that this guy was quiet and seemed conservative. The tag line just didn't fit, but I still think it was intentionalrosanna gusler wrote:I was wrong. Invisable shield. Our local grocery is the foodorama. Their slogan is "you can't beat our meat ".Marty wrote:That's a great name. Calls to mind another era, before focus groups.
Like Rosanna's Glassorama?
Dana W.