repairing kiln shelf

Post by ironman55 »

I have a Corelite shelf 1"X24X39 I heated up my kiln too fast (I think) it cracked full length completely. Can it be repaired with a high temp cement mortar or ???
Also, I cant find any company info on Corelite manufacturer. I would like to contact the company that actually makes them to ask their thoughts.

THanks for any help, Joe
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: repairing kiln shelf

Post by Brad Walker »

I don't believe the shelves can easily be repaired, but these are the guys that make the Core-lite shelves: http://www.rescoproducts.com/

Try calling Kevin Frederes or Eric Nedreberg, Resco Products Inc, 888-283-5505, Kevin.Frederes@rescoproducts.com, eric.nedreberg@rescoproducts.com
ironman55
Posts: 23
Joined: Tue Dec 30, 2014 2:02 pm

Re: repairing kiln shelf

Post by ironman55 »

Brad, Thanks for the info. I am sending an email.
Joe
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: repairing kiln shelf

Post by Judd »

If you can't repair it, then you can cut them into pattern bar molds.
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: repairing kiln shelf

Post by Havi »

Judd wrote:If you can't repair it, then you can cut them into pattern bar molds.
OR

cut them for damming


Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: repairing kiln shelf

Post by Havi »

Judd wrote:If you can't repair it, then you can cut them into pattern bar molds.
OR

cut them for damming


Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Sean McFeely
Posts: 3
Joined: Thu Jul 23, 2015 9:52 am

Re: repairing kiln shelf

Post by Sean McFeely »

You will be hard pressed to make a good repair. You can cast a new shelf using a Castable 3000 cement. It is good option for making fixtures if you don't mind a rougher surface. A good reminder to bake out moisture slowly after having your kiln in hibernation for a while.