Kiln wash turning brown and smoking?

Postby Bharr » Wed Jun 03, 2015 3:43 pm

I have been fusing for many years. I have been using Primo Hotline. I recently switched to Bullseye. It has worked fine, but all of a sudden it turns brown and starts smoking. Any ideas?

Judd
Posts: 291
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: Kiln wash turning brown and smoking?

Postby Judd » Thu Jun 04, 2015 11:21 am

It does this while firing, but after firing, it looks normal, right? If so, it's just the binders burning out.
Disclaimer: this is what I was told. I make my own kiln wash.

Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Kiln wash turning brown and smoking?

Postby Bert Weiss » Thu Jun 04, 2015 12:29 pm

The problem is that Bullseye kiln wash utilizes EPK for it's binder and EPK is clay with no organics. The only organic material in the BE wash would be the pink coloring. On the other hand, Primo uses an organic binder which would turn brown and then burn out.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Kiln wash turning brown and smoking?

Postby Valerie Adams » Thu Jun 04, 2015 7:36 pm

My Bullseye wash doesn't turn color or smoke.

Are you using fiber paper (like Thinfire) over the wash? I know Thinfire turns brown before returning to white, as the binders burn off.

Mark Kemp
Posts: 59
Joined: Mon Mar 10, 2003 11:57 am
Location: Corvallis, Oregon
Contact:

Re: Kiln wash turning brown and smoking?

Postby Mark Kemp » Fri Jun 05, 2015 4:17 am

Weird. I've never seen the BE wash turn color, smoke, or emit any odor. Could it have gotten contaminated somehow? Something in the mixing container? Did it get moldy?
Find peace in your heart.

www.azurefire.etsy.com

Andrea R
Posts: 61
Joined: Fri Sep 30, 2005 10:52 am
Location: Canada

Re: Kiln wash turning brown and smoking?

Postby Andrea R » Fri Jun 05, 2015 2:46 pm

agree my BE wash has never turned color or has it smoked.
Image
"C'est Moi (Its Me)"


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 50 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com