My friend Ruthie is a photographer.
Upon talking about printing on glass, she asked me if it will be possible to print a photograph of hers on glass, and will it be transparent [with colors] as glass.
My assumption is that this relates to the quality of the print / inking print. Whether it is transparent or opaque.
Am I right?
Are there at all printing inks for glass that are transparent?
We shall be very thankful for your response.
Havi
Printing on glass - - -
Moderators: Brad Walker, Tony Smith
Printing on glass - - -
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
-
Mike Jordan
- Posts: 94
- Joined: Mon Nov 06, 2006 11:13 pm
- Location: Hillsboro, OR
- Contact:
Re: Printing on glass - - -
You could turn it into a decal and then fuse the decal onto the glass, Havi. I did that a while back with some of my photos. There is a place you upload your images to and they send you the decals. They can be black and white or color. Here is some examples of when I tried it to see what they would look like.

The above was on a piece of white glass.
This one was on a clear piece of glass.

This is what the sheet of decals look like (minus the ones I cut out to put on glass)

I believe this is the play I bought them from. He charges by the page of decals:
http://www.decals4artists.com/index.html
Hope this helps.
Mike

The above was on a piece of white glass.
This one was on a clear piece of glass.

This is what the sheet of decals look like (minus the ones I cut out to put on glass)

I believe this is the play I bought them from. He charges by the page of decals:
http://www.decals4artists.com/index.html
Hope this helps.
Mike
It's said that inside each of us is an artist trying to get out. Well mine got out... and I haven't seen him since.
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Printing on glass - - -
Havi
The transparent colors tend to be low fire, around 1050ºF. These colors are hard to come by these days. Fusemaster sells some. Ferro makes them, but does not export them to the USA. I think you can get them in Europe.
There was a company called Glassmasters that screen printed transparent and opaque enamels to reproduce stained glass windows in small panels. I found this picture.

The transparent colors tend to be low fire, around 1050ºF. These colors are hard to come by these days. Fusemaster sells some. Ferro makes them, but does not export them to the USA. I think you can get them in Europe.
There was a company called Glassmasters that screen printed transparent and opaque enamels to reproduce stained glass windows in small panels. I found this picture.

Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: Printing on glass - - -
Dear Mike and Bert,
Thanks a lot for your response and illustration.
The photos are wonderful!, The flowers look really beautiful, and the dog too, actually,
I'll pass your responses to Ruthie.
Thanks again,
Havi.
Thanks a lot for your response and illustration.
The photos are wonderful!, The flowers look really beautiful, and the dog too, actually,
I'll pass your responses to Ruthie.
Thanks again,
Havi.
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
Re: Printing on glass - - -
Hi Havi, I haven't tried this process myself but have this site bookmarked...it seems close to what you're looking for.
http://www.decals4artists.com/index.html
http://www.decals4artists.com/index.html