Kaiser Lee Board where to buy??/
Moderator: Brad Walker
Kaiser Lee Board where to buy??/
I read with interest the discussion on using what sound great -Kaiser Lee Board.  I went to the website given but was unable to email, it was like a link but not email address.    
 Thanks for the help.  Pam
			
			
									
						
										
						- 
				Helen Stokes
 - Posts: 6
 - Joined: Sun Aug 24, 2003 6:15 pm
 - Location: Melbourne Australia
 - Contact:
 
Hi, try kaiserlee@earthlink.net
			
			
									
						
										
						- 
				Tony Smith
 - Posts: 1037
 - Joined: Sun Mar 09, 2003 5:59 pm
 - Location: Massachusetts, USA
 - Contact:
 
- 
				Robyn Alexander
 - Posts: 22
 - Joined: Fri Jul 04, 2003 7:49 pm
 - Location: Berkeley CA
 
CR Loo carries it as well.   
http://www.crloo.com
			
			
									
						
										
						http://www.crloo.com