I have been fusing jewelry for several years and now would like to try experimenting with decals.
I was wondering if I can be successful without having a controller on my kiln.
Any comments/suggestions and sources to purchase decals.
Thanks in advance.
			
			
									
						
										
						Decals
Moderator: Tony Smith
- 
				Barry Kaiser
 - Posts: 311
 - Joined: Mon Jul 25, 2005 6:54 pm
 - Location: North Carolina
 - Contact:
 
Re: Decals
Sure,
Decals come in high fire and low fire.
Just bring the temperature of your kiln to the level required by the type and turn off the kiln. You are done.
Note" if there is red or gold on the decal, vent(open the kiln lid slightly) it up to 1000°F.
Barry
			
			
									
						
							Decals come in high fire and low fire.
Just bring the temperature of your kiln to the level required by the type and turn off the kiln. You are done.
Note" if there is red or gold on the decal, vent(open the kiln lid slightly) it up to 1000°F.
Barry
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
			
						http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns